Polymer Property : Tensile Stress = 57.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 57.8 MPa

@Strain 8.80 %,
Temperature 40.0 °C
8380 psi

@Strain 8.80 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem..
Tensile Stress 57.8 MPa

@Strain 0.700 %,
Temperature 23.0 °C
8380 psi

@Strain 0.700 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers