Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 58.25 MPa @Strain 18.48 %, Temperature 0.000 °C |
8448 psi @Strain 18.48 %, Temperature 32.0 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |