Mechanical Properties Metric English Comments
Tensile Stress 58.39 MPa

@Strain 3.39 %,
Temperature 150 °C
8469 psi

@Strain 3.39 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® RE5264 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
36% Glass Reinforced Polyethylene Terephthalate Rynite RE5264 NC010 is a 36% glass fiber reinforced color stabilized modified polyethylene terephthalate.Information provided by DuPont Performance Po..
Tensile Stress 58.39 MPa

@Strain 4.74 %,
Temperature 23.0 °C
8469 psi

@Strain 4.74 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 153HSL NC010 Nylon 612  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers