Tensile Stress 40.9 MPa

@Strain 5.08 %,
Temperature 23.0 °C
5930 psi

@Strain 5.08 %,
Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers