Mechanical Properties Metric English Comments
Tensile Stress 60.7 MPa

@Thickness 0.0500 mm
8800 psi

@Thickness 0.00197 in
MD, Break; ASTM D882
Topas Advanced Polymers TOPAS® Elastomer E-140 Developmental Cyclic Olefin Copolymer (COC)
TOPAS® Elastomer E-140, unlike most TOPAS grades, is a semicrystalline cyclic olefin material with flexibility. It is a fairly stiff elastomer which can be extruded and injection molded, and can be..
Tensile Stress 60.7 MPa

@Strain 4.24 %,
Temperature 120 °C
8800 psi

@Strain 4.24 %,
Temperature 248 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66
Information provided by DuPont Performance Polymers