Mechanical Properties Metric English Comments
Tensile Stress 60.93 MPa

@Strain 7.09 %,
Temperature 150 °C
8837 psi

@Strain 7.09 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® GW520CS NC010 Polyethylene Terephthalate (PET)
20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified pol..