Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.15 MPa @Strain 196.33 %, Temperature 120 °C |
602 psi @Strain 196.33 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 4.15 MPa @Strain 0.120 %, Temperature 150 °C |
602 psi @Strain 0.120 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performan.. |
|||
Tensile Stress | 4.15 MPa @Strain 100.59 %, Temperature 100 °C |
602 psi @Strain 100.59 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |