Mechanical Properties Metric English Comments
Tensile Stress 62.48 MPa

@Strain 3.89 %,
Temperature 90.0 °C
9062 psi

@Strain 3.89 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf..