Polymer Property : Tensile Stress = 620 psi
Polymer Property :
Tensile Stress =
620 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Stress
4.27
MPa
@Strain 300 %
620
psi
@Strain 300 %
NEU NeuSoft™ 596-60A Medical Ether TPU / SBC blend