Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 63.23 MPa @Strain 5.00 %, Temperature 150 °C |
9171 psi @Strain 5.00 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G35HSL BK262 is a 35% glass fiber reinforced heat stabilized black polyamide 6 resin for injection molding.Information provided by DuPont Per.. |
|||
Tensile Stress | 63.23 MPa @Strain 0.460 %, Temperature 40.0 °C |
9171 psi @Strain 0.460 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G45DH2 BK083 is a 45% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |