Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 65.14 MPa @Strain 0.940 %, Temperature 60.0 °C |
9448 psi @Strain 0.940 %, Temperature 140 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK609 NC010 PBT
(Unverified Data**) Crastin® SK609 NC010 is a 50% glass fiber reinforced, lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 65.14 MPa @Strain 0.990 %, Temperature 90.0 °C |
9448 psi @Strain 0.990 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G45L NC010 Nylon 6
(Unverified Data**) 45% Glass Reinforced Polyamide 6Zytel 73G45L NC010 is a 45% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |