Polymer Property : Tensile Stress = 65.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 65.9 MPa

@Strain 8.00 %,
Temperature 23.0 °C
9560 psi

@Strain 8.00 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 900P BK602 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer with Improved ProcessingDelrin 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing t..
Tensile Stress 65.9 MPa

@Strain 7.80 %,
Temperature 23.0 °C
9560 psi

@Strain 7.80 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider..
Tensile Stress 65.9 MPa

@Strain 1.60 %,
Temperature 23.0 °C
9560 psi

@Strain 1.60 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 12T NC010 Nylon 66  (Unverified Data**)
36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T NC010 is a 36% mineral reinforced toughened heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performan..