Polymer Property : Tensile Stress = 658 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 4.54 MPa

@Strain 14.19 %,
Temperature 0.000 °C
658 psi

@Strain 14.19 %,
Temperature 32.0 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 4.54 MPa

@Strain 0.100 %,
Temperature 0.000 °C
658 psi

@Strain 0.100 %,
Temperature 32.0 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® FR7026V0F NC010 Nylon 66  (Unverified Data**)
Zytel® FR7026V0F NC010 is a flame retardant, heat stabilized, polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by D..