Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 45.72 MPa @Strain 2.83 %, Temperature -40.0 °C |
6631 psi @Strain 2.83 %, Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC4601 NC010 Nylon
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide Developed for Extrusion Zytel RS LC4601 NC010 is a flexible toughened and plasticized polyamide resin intended for extrusion applications.Informatio.. |