Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 67.81 MPa @Strain 2.86 %, Temperature 40.0 °C |
9835 psi @Strain 2.86 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene.. |
|||
Tensile Stress | 67.81 MPa @Strain 2.86 %, Temperature 40.0 °C |
9835 psi @Strain 2.86 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5315HFS NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene.. |