Polymer Property : Tensile Stress = 685 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 4.72 MPa

@Strain 100 %
685 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® D6865 TPE, Extruded
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from..
Tensile Stress 4.72 MPa

@Strain 0.230 %,
Temperature 0.000 °C
685 psi

@Strain 0.230 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo..
Tensile Stress 4.72 MPa

@Strain 118 %,
Temperature 90.0 °C
685 psi

@Strain 118 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers