Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.59 MPa @Strain 215.82 %, Temperature 120 °C |
1100 psi @Strain 215.82 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |