Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 70.86 MPa @Strain 1.75 %, Temperature 90.0 °C |
10280 psi @Strain 1.75 %, Temperature 194 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK609 NC010 PBT