Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.92 MPa @Strain 300 % |
714 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® A9870 TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |