Polymer Property : Tensile Stress = 72.39 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 72.39 MPa

@Strain 0.770 %,
Temperature -40.0 °C
10500 psi

@Strain 0.770 %,
Temperature -40.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610
30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Zytel RS 30G30L NC010 is a lubricated 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewabl..