Mechanical Properties Metric English Comments
Tensile Stress 73.0 MPa

@Strain 4.00 %,
Temperature 23.0 °C
10600 psi

@Strain 4.00 %,
Temperature 73.4 °F
ISO 527
BASF Ultrason E 3010 PES
Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance.