Mechanical Properties Metric English Comments
Tensile Stress 73.007 MPa

@Strain 0.700 %,
Temperature -40.0 °C
10589 psi

@Strain 0.700 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on pol..
Tensile Stress 73.007 MPa

@Strain 0.700 %,
Temperature -40.0 °C
10589 psi

@Strain 0.700 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo..