Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 50.6 MPa @Thickness 0.125 mm |
7340 psi @Thickness 0.00492 in |
TD, Break; ASTM D882 |
Topas Advanced Polymers TOPAS® Elastomer E-140 Developmental Cyclic Olefin Copolymer (COC) TOPAS® Elastomer E-140, unlike most TOPAS grades, is a semicrystalline cyclic olefin material with flexibility. It is a fairly stiff elastomer which can be extruded and injection molded, and can be.. |
|||
Tensile Stress | 50.61 MPa @Strain 0.330 %, Temperature 23.0 °C |
7340 psi @Strain 0.330 %, Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK609 NC010 PBT
(Unverified Data**) Crastin® SK609 NC010 is a 50% glass fiber reinforced, lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 50.6 MPa @Strain 17.8 %, Temperature 23.0 °C |
7340 psi @Strain 17.8 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 520MP NC010 Acetal (POM)
(Unverified Data**) 20% Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 520MP is a medium viscosity acetal homopolymer containing 20% Teflon PTFE Micropowder. It is designe.. |
|||
Tensile Stress | 50.61 MPa @Strain 0.890 %, Temperature 90.0 °C |
7340 psi @Strain 0.890 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® RE5264 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Glass Reinforced Polyethylene Terephthalate Rynite RE5264 NC010 is a 36% glass fiber reinforced color stabilized modified polyethylene terephthalate.Information provided by DuPont Performance Po.. |
|||
Tensile Stress | 50.6 MPa @Strain 0.900 %, Temperature 0.000 °C |
7340 psi @Strain 0.900 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |