Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 52.83 MPa @Strain 2.15 %, Temperature 90.0 °C |
7662 psi @Strain 2.15 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G35EF BK420 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN54G35EF BK420 is a 35% glass reinforced toughened heat stabilized lubrica.. |
|||
Tensile Stress | 52.83 MPa @Strain 2.70 %, Temperature 150 °C |
7662 psi @Strain 2.70 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G40DH1T BK261 Nylon
(Unverified Data**) Zytel® PLS95G40DH1T is a 40% GR impact modified PA, made with SHIELD technology, its superior heat & oil resistance combined with the "stone impact resistance" makes it ideal choice for use in seve.. |