Polymer Property : Tensile Stress = 7713 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 53.18 MPa

@Strain 4.05 %,
Temperature 150 °C
7713 psi

@Strain 4.05 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G33HS1L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin with outstanding impact resistance developed usin..
Tensile Stress 53.18 MPa

@Strain 4.52 %,
Temperature -40.0 °C
7713 psi

@Strain 4.52 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612  (Unverified Data**)
Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers