Tensile Stress 5.32 MPa

@Strain 0.230 %,
Temperature -40.0 °C
772 psi

@Strain 0.230 %,
Temperature -40.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612  (Unverified Data**)
Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers