Polymer Property : Tensile Stress = 779 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 5.37 MPa

@Strain 0.240 %,
Temperature -40.0 °C
779 psi

@Strain 0.240 %,
Temperature -40.0 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010  (Unverified Data**)
Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s..