Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.24 MPa @Strain 50.54 %, Temperature 60.0 °C |
1200 psi @Strain 50.54 %, Temperature 140 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin.. |