Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 8032 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 55.38 MPa

@Strain 2.19 %,
Temperature 150 °C
8032 psi

@Strain 2.19 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FR52G30NH BK337 Polyphthalamide (PPA)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It..
Tensile Stress 55.38 MPa

@Strain 2.90 %,
Temperature -20.0 °C
8032 psi

@Strain 2.90 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® ST830FRUV NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Flame Retardant UV Stabilized Polybutylene Terephthalate Crastin ST830FRUV NC010 is an unreinforced Super Tough flame retardant polybutylene terephthalate resin for injection molding. I..
Copyright © lookpolymers.com All Rights Reserved