Mechanical Properties Metric English Comments
Tensile Stress 81.52 MPa

@Strain 2.17 %,
Temperature 23.0 °C
11820 psi

@Strain 2.17 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66  (Unverified Data**)
Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du..
Tensile Stress 81.52 MPa

@Strain 8.65 %,
Temperature 90.0 °C
11820 psi

@Strain 8.65 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 53G50HSLR NC010 Polyphthalamide (PPA)  (Unverified Data**)
50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR NC010 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve..