Polymer Property : Tensile Stress = 8180 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 56.4 MPa

@Strain 2.50 %,
Temperature 23.0 °C
8180 psi

@Strain 2.50 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 311DP BK402 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP BK402 is a medium high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced..
Tensile Stress 56.4 MPa

@Strain 2.20 %,
Temperature 0.000 °C
8180 psi

@Strain 2.20 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s..
Tensile Stress 56.4 MPa

@Strain 2.20 %,
Temperature 0.000 °C
8180 psi

@Strain 2.20 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo..
Tensile Stress 56.4 MPa

@Strain 0.350 %,
Temperature 23.0 °C
8180 psi

@Strain 0.350 %,
Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Rynite® FR543 NC010 PET
Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm..