Mechanical Properties Metric English Comments
Tensile Stress 82.32 MPa

@Strain 9.00 %,
Temperature -20.0 °C
11940 psi

@Strain 9.00 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider..