Tensile Stress 5.71 MPa

@Strain 0.0400 %,
Temperature 23.0 °C
828 psi

@Strain 0.0400 %,
Temperature 73.4 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66  (Unverified Data**)
Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in..