Mechanical Properties Metric English Comments
Tensile Stress 57.84 MPa

@Strain 5.03 %,
Temperature 90.0 °C
8389 psi

@Strain 5.03 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK602 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Polybutylene Terephthalate Crastin SK602 NC010 is a 15% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..