Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 85.24 MPa @Strain 0.800 %, Temperature 23.0 °C |
12360 psi @Strain 0.800 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66
(Unverified Data**) Zytel® 80G43HS1L BK104 is a 43% glass fiber reinforced, heat stabilized, black polyamide 66 resin with superior impact resistance.Information provided by DuPont Performance Polymers |