Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 85.54 MPa @Strain 0.810 %, Temperature -40.0 °C |
12410 psi @Strain 0.810 %, Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G30NH NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |