Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 86.98 MPa @Strain 1.00 %, Temperature 40.0 °C |
12620 psi @Strain 1.00 %, Temperature 104 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK609 NC010 PBT