Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 59.6 MPa

@Strain 4.00 %,
Temperature 23.0 °C
8640 psi

@Strain 4.00 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500P BK602 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Improved ProcessingDelrin 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin 500P has improved pro..
Tensile Stress 59.6 MPa

@Strain 0.710 %,
Temperature 0.000 °C
8640 psi

@Strain 0.710 %,
Temperature 32.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G33HS1L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin with outstanding impact resistance developed usin..
Tensile Stress 59.6 MPa

@Strain 14.4 %,
Temperature 40.0 °C
8640 psi

@Strain 14.4 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and ..