Polymer Property : Tensile Stress = 872 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 6.01 MPa

@Strain 100.76 %,
Temperature 150 °C
872 psi

@Strain 100.76 %,
Temperature 302 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 6.01 MPa

@Strain 0.250 %,
Temperature -20.0 °C
872 psi

@Strain 0.250 %,
Temperature -4.00 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1610 BK387 Nylon 1010  (Unverified Data**)
Plasticized Toughened Renewably Sourced Polyamide 1010 Developed for Extrusion Information provided by DuPont Performance Polymers
Tensile Stress 6.01 MPa

@Strain 50.52 %,
Temperature 100 °C
872 psi

@Strain 50.52 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET  (Unverified Data**)
44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin..