Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 60.167 MPa @Strain 0.900 %, Temperature 0.000 °C |
8726.5 psi @Strain 0.900 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® IG38C1 BK434 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon IG38C1 BK434 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |