Mechanical Properties Metric English Comments
Tensile Stress 6.18 MPa

@Strain 300 %
896 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® C4945 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress 6.18 MPa

@Strain 17.14 %,
Temperature 150 °C
896 psi

@Strain 17.14 %,
Temperature 302 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers