Polymer Property : Tensile Stress = 9.00 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 7.00 - 9.00 MPa

@Strain 100 %
1020 - 1310 psi

@Strain 100 %
TM-019G
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets
Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc...
Tensile Stress 7.00 - 9.00 MPa

@Strain 100 %
1020 - 1310 psi

@Strain 100 %
TM-019G
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets
Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc...