Polymer Property : Tensile Stress = 911 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 6.28 MPa

@Strain 4.92 %,
Temperature 150 °C
911 psi

@Strain 4.92 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610  (Unverified Data**)
Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by..
Tensile Stress 6.28 MPa

@Strain 187.51 %,
Temperature 180 °C
911 psi

@Strain 187.51 %,
Temperature 356 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET  (Unverified Data**)
65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers