Mechanical Properties Metric English Comments
Tensile Stress 0.640 MPa

@Strain 0.000 %,
Temperature 200 °C
92.8 psi

@Strain 0.000 %,
Temperature 392 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66  (Unverified Data**)
Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in..
Tensile Stress 0.640 MPa

@Strain 0.200 %,
Temperature 90.0 °C
92.8 psi

@Strain 0.200 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET  (Unverified Data**)
65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers