Tensile Stress 6.35 MPa

@Strain 7.08 %,
Temperature 100 °C
921 psi

@Strain 7.08 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 6.35 MPa

@Strain 1.21 %,
Temperature 150 °C
921 psi

@Strain 1.21 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6  (Unverified Data**)
30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro..