Mechanical Properties Metric English Comments
Tensile Stress 64.96 MPa

@Strain 6.96 %,
Temperature 150 °C
9422 psi

@Strain 6.96 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610
30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Zytel RS 30G30L NC010 is a lubricated 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewabl..
Tensile Stress 64.96 MPa

@Strain 1.07013 %,
Temperature -40.0 °C
9422 psi

@Strain 1.07013 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK612SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
15% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK612SF is a 15% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..