Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 65.806 MPa @Strain 3.2535 %, Temperature 60.0 °C |
9544.4 psi @Strain 3.2535 %, Temperature 140 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 510GR NC000 Acetal Homopolymer
(Unverified Data**) Delrin® 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength, stiffness, and high deflection temperature and excellent creep resistance.Information provide.. |