Polymer Property : Tensile Stress = 96.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 96.2 MPa

@Strain 3.47 %,
Temperature 40.0 °C
14000 psi

@Strain 3.47 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6  (Unverified Data**)
30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performan..