Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 66.49 MPa

@Strain 0.460 %,
Temperature 23.0 °C
9644 psi

@Strain 0.460 %,
Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Crastin® SK609 NC010 PBT  (Unverified Data**)
Crastin® SK609 NC010 is a 50% glass fiber reinforced, lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers