Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 6.67 MPa @Strain 100 % |
967 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® F02-081A-6C TPE, Halogen Free Extrusion Grade Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to.. |
|||
Tensile Stress | 6.67 MPa @Strain 4.80 %, Temperature 150 °C |
967 psi @Strain 4.80 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 6.67 MPa @Strain 4.80 %, Temperature 150 °C |
967 psi @Strain 4.80 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for .. |